The Story
- Japan AGC Asahi Glass
- 3X times reinforced treatment
- Pressure test around 20-35kg
- Oleophilic coating
- Light transmittance around  92%
- 1M solid ball drop test passed
- Anti-dust adhesive adopted for free bubble
- Standard Friction of Glass surface test reaches 10000 times
Description
- Japan AGC Asahi Glass
- 3X times reinforced treatment
- Pressure test around 20-35kg
- Oleophilic coating
- Light transmittance around  92%
- 1M solid ball drop test passed
- Anti-dust adhesive adopted for free bubble
- Standard Friction of Glass surface test reaches 10000 times